Processing and Mechanical Properties of 30vol%TiC\-p/W Composite
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    研究了烧结温度,烧结保温时间和烧结压力等工艺参数对各30%TiC(体积分数,下同)颗粒的钨基复合材料的力学性能的影响,得到了制备30%TiCp/W复合材料的优化的热压烧结工艺为:2000℃,20MPa压力下烧结60min,用优化工艺制备的30%TiCp/W复合材料的高温强度比其室温强度要高,这种极好高温强度主要是由于W基体随温度上升发生了由脆性到塑性的转变,使TiC颗粒的增强效果在高温得以充分发挥

    Abstract:

    The effects of sintering temperature,holding time and hot pressure on the density and mechanical properties of a hot pressed(PM)powder metallurgy 30vol%TiC\-p/W composite have been investigated. An optimum process for the preparation of 30vol%TiC\-p/W composite with higher strength and toughness has been devised.The 30vol%TiC\-p/W composite has excellent high temperature strength.This is attributed to a brittle ductile transision of the tungsten matrix combined with the strengthening effect of hard TiC particles in the W matrix.

    参考文献
    相似文献
    引证文献
引用本文

宋桂明 周玉. TiCp/W复合材料的制备工艺与力学性能[J].稀有金属材料与工程,1999,(3):171~175.[Song Guiming, Zhou Yu, Wang Yujin, Lei Tingquan. Processing and Mechanical Properties of 30vol%TiC\-p/W Composite[J]. Rare Metal Materials and Engineering,1999,(3):171~175.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期:
  • 出版日期: