Effect of Oxygen Impurity and Overheating on Microstructure and MechanicalProperties of As-cast Zr52.5Cu17.9Ni14.6Al10Tis Bulky Glass Alloys
Clc Number:

TG139.8

  • Article
  • | |
  • Metrics
  • | |
  • Related [20]
  • | | |
  • Comments
    Reference
    Cited by
    Comments
    Comments
    分享到微博
    Submit
Get Citation

[. Effect of Oxygen Impurity and Overheating on Microstructure and MechanicalProperties of As-cast Zr52.5Cu17.9Ni14.6Al10Tis Bulky Glass Alloys[J]. Rare Metal Materials and Engineering,2001,(3):190~193.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:1481