    Abstract:

    The preparation and formability of 30W-Cu EFP(explosively formed projectile) liner were studied. At first the two different 30W-Cu materials were prepared by tungsten powder, copper powder and ultrafine tungsten-copper composite powder, and then the two materials’ formability were tested. Finally the material which had good formability was used to prepare EFP liner. It was found that the 30W-Cu material prepared by common tungsten powder and copper powder had a good formability. 98.2% of the theoretical density of the density of the 30W-Cu EFP liner material was obtained. After annealing, the tensile strength of the material reached 315 MPa and elongation reached 15.3%

    Reference
    Related
    Cited by
Get Citation

[Zhang Quanxiao, Yao Dong, Cao Lianzhong, Jia Wanming, Ma Shaohua, Zhao Hongmei. Preparation and Formability of Tungsten-Copper EFP Liner[J]. Rare Metal Materials and Engineering,2009,38(3):527~531.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:February 25,2008
  • Revised:
  • Adopted:
  • Online:
  • Published: