    Blue persistent luminescent β-Ga2O3: B3+ was synthesized by high solid-state reaction. The phosphor exhibits more than 0.5 h afterglow in the wavelength range of 380-600 nm after ceasing the ultraviolet light (260 nm) irradiation. The emission and excitation spectra, persistent luminescence decay curve, and thermoluminescence curve were measured. The emission and excitation spectra indicate that the B3+ doping improves on photoluminescent properties of β-Ga2O3. The thermoluminescence (TL) curve of β-Ga2O3: 80% B3+ shows that B3+ increased the traps and improved the depth of the traps.

    Reference
    Related
    Cited by
Get Citation

[Ruixia Zhong, Jianquan Qi, Ziran Liu. Long-lasting blue persistent luminescence from β-Ga2O3 with B3+ addition[J]. Rare Metal Materials and Engineering,2018,47(S1):78~82.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:May 25,2017
  • Revised:July 07,2017
  • Adopted:January 29,2018
  • Online: October 22,2018
  • Published: